High Alloy Heat-resistant Castings
Highly alloy heat and abrasion resistant castings can effectively resist heat, wear and oxidation in different temperature ranges within 600~1300℃.
The main products include spraying nozzles of boilers, grate barsfor sintering, grate plates for clinker cooling machines, furnace bed platesand teeth for slag crushers.
Material |
Endurance strength(Mpa) 1000℃ 1000hr |
Oxidation weight gain (g/m2) 1000℃ 500hr |
Temperature range applicable |
30Cr26Ni14Si2MoNRENb | ≥16 | ≤50 | 800—1300℃ |
40Cr25Ni20 | ≥10 | ≤50 | 800—1300℃ |
35Cr18Ni25Si2 | ≥8 | ≤65 | 800—1300℃ |
30Cr22Ni4Mn4Si2N | ≥8 | ≤115 | 600—1300℃ |